This Aluminized steel end of a catalytic converter is formed in a one station die. Split rejects were over 50% until Ameriform.The reject rate is less than .001% at present
j
Forming Examples
This stainless Transmission clutch housing is the only lube capable of consistently producing a quality part. Forming film thickness of 175 mil grams/ft2 (less than .1 mil). r
HDG .054 Inner Pillar Before Ameriform the reject rate was close to 100%. After changing to Ameriform as the forming dry film lube, there were no rejects